• Tittanium Bar Materials: Grade1, Grade 2, Grade 5, Grade 5, Grade7 ,Grade9,Grade11, Grade12, Grade 16, Grade23 ect
• Bar Shapes: Round Bar, Flat Bar, Hex Bar, Square bar
• Diameter:2.0mm-320mm, Length: 50mm-6000mm, Customized
• Conditions: Hot Forging & Hot Rolling,Cold Rolled, Annealed
• Standards: ASTMB348, AMS4928, AMS 4931B, ASTM F67, ASTM F136 etc
Titanium Alloys Material Common Name | ||
Gr1 |
UNS R50250 |
CP-Ti |
Gr2 |
UNS R50400 |
CP-Ti |
Gr4 |
UNS R50700 |
CP-Ti |
Gr7 |
UNS R52400 |
Ti-0.20Pd |
G9 |
UNS R56320 |
Ti-3AL-2.5V |
G11 |
UNS R52250 |
Ti-0.15Pd |
G12 |
UNS R53400 | Ti-0.3Mo-0.8Ni |
G16 |
UNS R52402 | Ti-0.05Pd |
G23 |
UNS R56407 |
Ti-6Al-4V ELI |
Grade |
Chemical composition, weight percent (%) |
||||||||||||
C (≤) |
O (≤) |
N (≤) |
H (≤) |
Fe (≤) |
Al |
V |
Pd |
Ru |
Ni |
Mo |
Other Elements Max. each |
Other Elements Max. total |
|
Gr1 |
0.08 |
0.18 |
0.03 |
0.015 |
0.20 |
— |
— |
— |
— |
— |
— |
0.1 |
0.4 |
Gr2 |
0.08 |
0.25 |
0.03 |
0.015 |
0.30 |
— |
— |
— |
— |
— |
— |
0.1 |
0.4 |
Gr4 |
0.08 |
0.25 |
0.03 |
0.015 |
0.30 |
— |
— |
— |
— |
— |
— |
0.1 |
0.4 |
Gr5 |
0.08 |
0.20 |
0.05 |
0.015 |
0.40 |
5.5 6.75 |
3.5 4.5 |
— |
— |
— |
— |
0.1 |
0.4 |
Gr7 |
0.08 |
0.25 |
0.03 |
0.015 |
0.30 |
— |
— |
0.12 0.25 |
— |
0.12 0.25 |
— |
0.1 |
0.4 |
Gr9 |
0.08 |
0.15 |
0.03 |
0.015 |
0.25 |
2.5 3.5 |
2.0 3.0 |
— |
— |
— |
— |
0.1 |
0.4 |
Gr11 |
0.08 |
0.18 |
0.03 |
0.15 |
0.2 |
— |
— |
0.12 0.25 |
— |
— |
— |
0.1 |
0.4 |
Gr12 |
0.08 |
0.25 |
0.03 |
0.15 |
0.3 |
— |
— |
— |
— |
0.6 0.9 |
0.2 0.4 |
0.1 |
0.4 |
Gr16 |
0.08 |
0.25 |
0.03 |
0.15 |
0.3 |
— |
— |
0.04 0.08 |
— |
— |
— |
0.1 |
0.4 |
Gr23 |
0.08 |
0.13 |
0.03 |
0.125 |
0.25 |
5.5 6.5 |
3.5 4.5 |
— |
— |
— |
— |
0.1 |
0.1 |
Grade |
Physical properties |
|||||
Tensile strength Min |
Yield strength Min (0.2%,offset) |
Elongation in 4D Min (%) |
Reduction of Area Min (%) |
|||
ksi |
MPa |
ksi |
MPa |
|||
Gr1 |
35 |
240 |
20 |
138 |
24 |
30 |
Gr2 |
50 |
345 |
40 |
275 |
20 |
30 |
Gr4 |
80 |
550 |
70 |
483 |
15 |
25 |
Gr5 |
130 |
895 |
120 |
828 |
10 |
25 |
Gr7 |
50 |
345 |
40 |
275 |
20 |
30 |
Gr9 |
90 |
620 |
70 |
483 |
15 |
25 |
Gr11 |
35 |
240 |
20 |
138 |
24 |
30 |
Gr12 |
70 |
483 |
50 |
345 |
18 |
25 |
Gr16 |
50 |
345 |
40 |
275 |
20 |
30 |
Gr23 |
120 |
828 |
110 |
759 |
10 |
15 |
• Grade 1: Pure Titanium, relatively low strength and high ductility.
• Grade 2: The pure titanium most used. The best combination of strength
• Grade 3: High strength Titanium, used for Matrix-plates in shell and tube heat exchangers
• Grade 5: The most manufactured titanium alloy. Exceedingly high strength. high heat resistance.
• Grade 7: Superior corrosion resistance in reducing and oxidizing environments.
• Grade 9: Very high strength and corrosion resistance.
• Grade 12: Better heat resistance than pure Titanium. Applications as for Grade 7 and Grade 11.
• Grade 23: Titanium-6Aluminum-4Vanadium ELI (Extra Low Interstitial) Alloy for surgical implant application.